Eck® Complete Corrosion Protection Test Results
Proven Through Thousands of Hours of Testing
Eck® Complete Corrosion Protection has undergone extensive laboratory and field testing to evaluate its ability to protect metal assemblies from corrosion, including galvanic corrosion caused by contact between dissimilar metals.
Laboratory testing shows Eck successfully passing a 4,000-hour test. Additional evaluations have included ASTM B117 salt spray testing conducted by manufacturers and laboratories across several industries. These tests have examined Eck in applications involving aluminum, steel, stainless steel, fasteners, hinges, compartment doors, and other assembled components.
CORROSION TESTING
E-ONE / DUPONT | 1,000-HOUR ASTM B117 TEST
E-One and DuPont conducted a 1,000-hour ASTM B117 salt spray evaluation using fire apparatus compartment doors. The test compared several corrosion-protection configurations, including Eck, Tef-Gel, and untreated assemblies.
Areas treated with Eck showed no reaction during laboratory exposure. For additional information on the test setup and findings, review the E-One/DuPont test report.
PPG INDUSTRIES | 1,000-HOUR ASTM B117 TEST
PPG Industries conducted a 1,000-hour ASTM B117 evaluation using commercial vehicle assemblies that combined dissimilar metals. Test panels included aluminum compartment doors, steel posts, hinges, bolts, and rivets.
The Eck-treated assemblies showed significant protection of the dissimilar metals with no visible corrosion following the test period. The PPG test documentation provides additional details on the test configuration and results.
GREAT DANE | 250-HOUR ASTM B117 COMPARISON
Great Dane's Research & Development laboratory evaluated two approaches for protecting a steel-to-aluminum assembly: Mylar Tape and Eck Corrosion Coating.
The test used steel and aluminum components secured with steel bolts, with Eck applied to drilled holes, fastener threads, and mating surfaces between the dissimilar metals. See the Great Dane test report for the complete comparison and test results.
SEYMOUR OF SYCAMORE | 400-HOUR ASTM B117 TEST
Seymour of Sycamore tested Eck on aluminum panels assembled with stainless steel hinges and bolts. Half of the test panels were left untreated while the remaining panels received Eck.
After 400 hours of salt spray exposure, the Eck-treated assemblies showed that the coating drastically reduced or stopped galvanic corrosion affecting the stainless-steel hinges and fasteners assembled with the aluminum panels. The Seymour of Sycamore test documentation provides complete results.
FLAMMABILITY TESTING
Eck has undergone flammability testing to evaluate its characteristics in a manufacturing environment. The results demonstrate that Eck is suitable for use in manufacturing facilities.
WHAT THE TESTING DEMONSTRATES
Taken together, these evaluations demonstrate Eck's performance across a range of materials, hardware configurations, and demanding vehicle applications, including:
• Aluminum and steel components
• Stainless steel hardware
• Fasteners, bolts, rivets, and hinges
• Commercial vehicle assemblies
• Fire apparatus components
• Truck and trailer applications
From extended laboratory exposure to application-specific evaluations, these results provide documented evidence of Eck's performance as a corrosion-protection coating.
Test results are an important consideration when evaluating a product's ability to provide critical corrosion protection across diverse applications. Austin Hardware can help you determine how to incorporate Eck into your manufacturing or assembly process based on the materials, hardware, and environmental conditions involved.